Your cart is empty.
Your cart is empty.A heavy-duty mold that holds up to 100 troy ounces of gold! Requires the use of a releasing agent - we recommend the Metallon Spray CAST-0027. Designed with a slight taper for easy ingot removal. Overall Dimensions: 9.75" Long x 3" Wide x 1.75" Deep. Bar Dimensions Flat Stock: 5.5" x 2.3125" x 1.25"
Brent
2025-08-27 13:21:55
Man this thing is BIG! My previous biggest mold was an 80 oz. A full aluminum bar is 0.8 lbs. Using this new hog of a mold a full bar is 1.7 lbs......more than twice the weight. Now THESE are bars. Can't wait to do copper in them. That's going to be a heavy bar. A little bumpy on the inside so I spent a lot of time with sand paper and a Dremel to smooth out the high spots and to get the paint off of it. Your first pour will make the bar all black from the paint. After sanding I made the mistake of rinsing it out with water to get all the powder out and it rusty some. Will now have to sand that out. Best to just wipe it out. All that said, this mold is awesome!!
Justin A.
2025-07-13 21:05:01
Not really sure what to write but i really like this item. Ive mostly melted lead in it. Or poured lead into it rather. Did some aluminum as well. It gets hot when full of liquid metal ofcpurse but has held up to multiple pourings. Ive made a dozen ingots and its just as fine as when i first got it. Obviously you gotta be careful with it so you dont break it but its a good item
Jason H.
2025-07-09 17:30:19
Sturdy and will not degrade like graphite molds. Also tapered so that the ingot slides out relatively easy. However, you should use an spray agent that allows easy separation.
greg
2025-07-04 14:47:39
Pretty good but already starting to degrade after several uses.
Hooziz
2025-07-01 09:53:01
The media could not be loaded.
Bradley Peacock
2025-05-22 18:14:43
This bad boy is solid and heavy! Molds come out great! Love it! Copper bars come out around 5 lbs of you top it off!
Major Consumer
2025-04-24 12:26:46
A chunk of the mold broke off and stuck to my ingot. It literally fused to the top of my second ingot when it dropped out of the mold. I took a closer look and it seems the base of the mold I received was incredibly thin for some reason. The walls of the mold seem nice and thick, but the base seems to about as thick as a U.S. nickel. Amazon refunded my purchase, but still, it was a let down to see the mold fail after only the second pour. Others seem to have no problem and cast many ingots, so I may have just received a random defective product. Good luck I guess.
Armando Duarte
2025-03-22 16:35:51
Much more durable than graphite, but the handle is weak....broke after 3 heat cycles. Must take your time in allowing to cool before picking up or the handle will crack/fall off.
Chuck
2025-02-03 17:40:34
Nice heavy retains heat.Not a fan of the paint on it but still give it a 5 star.